Know-how – XINDA https://www.xindacorp.com Co-Kneader, Twin Screw Extruder, and Compounding equipment Tue, 26 Aug 2025 10:32:45 +0000 en-US hourly 1 https://wordpress.org/?v=7.1.5 Co-rotating vs. Counter-rotating Twin-Screw Extruders https://www.xindacorp.com/co-rotating-vs-counter-rotating-twin-screw-extruders/ Tue, 26 Aug 2025 10:29:22 +0000 https://www.xindacorp.com/?p=4851

In polymer compounding, twin-screw extruders are essential for mixing, melting, and preparing materials. The direction in which the two screws rotate—either the same way or opposite ways—creates significant differences in performance. Xinda produce both the co-rotating and counter-rotating parallel twin screw extruder. Understanding these differences is key to selecting the right Xinda extruder for your product.

The Basic Difference

Imagine two screws side-by-side:

In a Co-rotating extruder, both screws rotate in the same direction. The material is pushed along in a figure-“∞” (infinity) path, passing easily between the screws.

In a Counter-rotating extruder, the screws rotate towards each other. The material is trapped in “C”-shaped chambers and is pushed forward more like a positive-displacement pump.

Key Performance Comparisons

Mixing Style:

Co-rotating: Excellent at distributive mixing. It spreads particles evenly throughout the melt, creating a very uniform blend. Think of it like perfectly folding egg whites into cake batter.

Counter-rotating: Excellent at dispersive mixing. It applies high shear and force to break down agglomerates, fillers, or pigments. Think of it like grinding peppercorns into a fine powder.

Material Conveying & Processing:

Co-rotating: Has a gentler shear and a more stable pressure profile. Materials move through it faster with a shorter, more consistent residence time. This is ideal for heat-sensitive polymers that might degrade if kept in the machine too long.

Counter-rotating: Has a stronger pumping action and can generate higher pressures, but can also create pressure peaks. Materials reside in the barrel for a longer and wider range of times, which is beneficial for processes that need longer reaction periods.

Final Product Properties:

The mixing style directly influences the final material’s characteristics:

Products from Co-rotating extruders often have better tensile strength and elongation due to the uniform distribution of ingredients.

Products from Counter-rotating extruders often have higher impact strength and lower melt viscosity because the intense shear breaks polymer chains more thoroughly.

So which One to Choose?

Use a Co-rotating extruder when you need a homogeneous mix, are working with heat-sensitive materials, or need high tensile properties in your final product.

Use a Counter-rotating extruder when you need to break down tough additives, achieve excellent dispersion, or need a longer reaction time inside the barrel for your process.

By matching the extruder’s strengths to your material’s requirements, you can optimize both your process efficiency and the quality of your final compounded product.

]]>
Introduction of Semi-Conductive Cable Compounds https://www.xindacorp.com/introduction-of-semi-conductive-cable-compounds/ Mon, 17 Jun 2024 08:13:06 +0000 https://www.xindacorp.com/?p=4501

Semi-conductive cable compounds are materials used in the production of power cables to provide certain electrical properties. They are formulated to have specific conductivity characteristics, typically designed to prevent the formation of electrical fields and ensure uniform distribution of electrical stress within the cable insulation.

Function and Introduction:

Semi-conductive cable compounds serve several functions in power cables:

  • Electrical Stress Control: They help in distributing electrical stress evenly across the cable insulation, reducing the risk of electrical breakdown.
  • Preventing Corrosion: These compounds often include additives to protect against corrosion and oxidation.
  • Environmental Protection: They provide resistance to environmental factors such as moisture and UV radiation.
  • Mechanical Stability: These compounds enhance the mechanical properties of the cable insulation, providing durability and strength.

Rough Formulation:

The formulation of semi-conductive cable compounds can vary depending on specific requirements and manufacturer preferences. However, a typical formulation may include:

  • Polymer Base: polyethylene (PE)
  • Carbon Black: To impart semi-conductive properties.
  • Additives: Including antioxidants, stabilizers, and processing aids.
  • Fillers: Such as mineral fillers for reinforcement and to control properties like density.

Compounding Requirements for Semi-conductive Cable Compounding:

Uniform Dispersion: Effective dispersion of carbon black or other conductive fillers within the polymer matrix is essential to ensure consistent electrical conductivity throughout the compound.

Stabilization: Incorporation of antioxidants and stabilizers to protect the compound from degradation due to heat, oxidation, and environmental factors, ensuring long-term performance and reliability.

Consistent Quality: Tight control over processing parameters such as temperature, mixing time, and shear rate is necessary to maintain batch-to-batch consistency and quality of the compound.

Processing Efficiency: Efficient mixing and dispersion are crucial to minimize processing time and energy consumption while maximizing throughput and productivity.

Compounding Process for Semi-conductive cable compounds:

Compounding: The raw materials, including the polymer base, carbon black, additives, and fillers, are mixed together in precise proportions in a compounding mixer. This process ensures uniform distribution of ingredients with XINDA Co-Kneader.

XINDA Semi-conductive cable compounding line
XINDA Semi-conductive cable compounding line
]]>
Introduction of HFFR Cable Compounds https://www.xindacorp.com/introduction-of-hffr-cable-compounds/ Tue, 06 Feb 2024 02:29:48 +0000 https://www.xindacorp.com/?p=4356

In the realm of cable technology, Halogen-Free Flame Retardant (HFFR) cable compounds play a crucial role in ensuring human safety. This article delves into the significance of HFFR in maintaining safety standards, the composition and manufacturing process of HFFR cable compounds, their diverse applications across industries, and the advantages of employing HFFR cables. Additionally, we will explore why the Xinda Co-Kneader compounding line stands out as an ideal choice for manufacturing HFFR cable compounds.

What is HFFR cable compounds?

HFFR stands for Halogen-Free Flame Retardant, a type of cable compound designed to limit the spread of fire and reduce smoke emission during a fire incident. Unlike traditional PVC cables that contain halogen-based materials, HFFR cables utilize flame retardant additives without halogen elements, minimizing potential hazards associated with halogen combustion.

HFFR cable_Halogen free flame retardant cable

The Importance of HFFR in Ensuring Human Safety:

Reduced Fire Spread: HFFR cables are engineered to resist combustion and slow down the spread of fire. This characteristic is pivotal in preventing the rapid propagation of flames in case of a fire incident, contributing significantly to the safety of occupants.

Low Smoke Emission: During a fire, smoke inhalation poses a severe threat to human health. HFFR cables produce minimal smoke when exposed to fire, improving visibility for evacuation efforts and reducing the respiratory risks associated with toxic smoke.

Compliance with Safety Standards: Many industries, especially those involving public spaces and critical infrastructure, adhere to stringent safety regulations. HFFR cables are designed to meet or exceed these standards, providing an added layer of assurance regarding human safety.

HFFR Formulation Ingredients:

HFFR cable compounds consist of a blend of polymers, flame retardant additives, and other materials. Common polymer matrices include polyethylene (PE), polypropylene (PP), and ethylene-vinyl acetate (EVA). Flame retardant additives like aluminum hydroxide and magnesium hydroxide are crucial for enhancing fire resistance. Usually, the ATH or MGH powder filling percentage will range from 55%~65% based on different formulation.

Manufacturing Process:

The production of HFFR cable compounds involves a meticulous process of compounding and extrusion. The raw materials are mixed in precise proportions using specialized equipment, such as the BUSS Kneader or Xinda Co-Kneader compounding line. This ensures uniform dispersion of additives and consistent cable performance.

XINDA HFFR Co-Kneader compounding line layout

Applications of HFFR Cables in Various Industries:

Construction Industry: HFFR cables are extensively used in construction for wiring and power distribution. Their flame-retardant properties are critical in minimizing the risk of fire in buildings.

Transportation Sector: In automotive and aerospace applications, where space is confined, the low smoke emission of HFFR cables becomes crucial. These cables are employed in vehicle wiring systems and aircraft interiors.

Telecommunications: The telecommunications industry utilizes HFFR cables to ensure reliable and safe data transmission. The flame-retardant nature of these cables is vital in preventing network failures caused by fire incidents.

Oil and Gas Exploration: Harsh environments in the oil and gas sector demand cables with robust fire resistance. HFFR cables find applications in drilling operations and offshore platforms.

Why Xinda Co-Kneader Compounding Line is Good for HFFR Cable Compounds:

Precision and Consistency: Since ATH and MDH filling materials have relatively narrow processing temperature, Xinda Co-Kneader compounding line excels in providing precise temperature control over the compounding process. Meanwhile Co-Kneader efficient and tender shear can ensure consistent dispersion of flame retardant additives in the cable compound.

High Throughput: This compounding line is known for its high throughput capabilities, allowing for efficient and large-scale production of HFFR cable compounds to meet industry demands.

Versatility: The Xinda Co-Kneader compounding line is versatile and can handle a wide range of polymer matrices and additives, making it suitable for the diverse formulations used in HFFR cable manufacturing.

Energy Efficiency: With advanced energy-efficient features, the Xinda Co-Kneader compounding line minimizes energy consumption during the manufacturing process, contributing to sustainability.

HFFR cable compounds stand as a pivotal innovation in the cable industry, prioritizing human safety by limiting fire hazards and minimizing smoke emissions. The composition, manufacturing process, and applications of HFFR cables underscore their importance in various industries. The advantages of using HFFR cables, coupled with the efficiency of the Buss Kneader and Xinda Co-Kneader compounding line, make a compelling case for the adoption of HFFR technology in cable manufacturing. As safety regulations become more stringent, the role of HFFR cables is poised to expand, ensuring a safer and more sustainable future across industries.

 

]]>
The factors of underwater cutter damage and the solutions https://www.xindacorp.com/how-to-control-pellet-moisture-with-underwater-pelletizer-2/ Sun, 28 Mar 2021 08:54:41 +0000 https://www.xindacorp.com/?p=3887 The factors of underwater cutter damage and improvement solutions are here!

In actual production, the underwater pelletizing equipment is prone to cutter damage, resulting in unqualified pellets, which not only increases the cost of cutter replacement, but also may cause customer quality complaints and economic losses.

Extending the service life of the cutter can not only ensure the appearance quality of granulation, but also save the material cost of the cutter, and at the same time reduce the number of stops of the extruder caused by the replacement of the cutter. Therefore, it is very necessary to study the factors affecting the service life of the cutter.

What is the cutter damage?

In long-term continuous production, different forms of cutter damage will occur, including cutter wear, cutter passivation and deformation, cutter breakage, etc. Among them, during normal production, the wear and passivation of the cutter is the most common phenomenon; when the production fluctuates, the cutter is prone to entanglement (see Figure 1), and cleaning the resin covering the cutter is easy to passivate and deform the blade . In order to prolong the service life of the cutter, special attention should be paid to the wear and tear of the cutter and the phenomenon of material sticking to the knife.

underwater pelletizer cutter

Influencing factors of cutter damage

1,Pelletizing process

The contact pressure of the cutter is regulated by the feeding air pressure and the returning air pressure. The feeding air pressure increases and the returning air pressure decreases. The closer the contact between the cutter and the die plate, the greater the friction between the cutter and the die plate, resulting in an increase in the current of the cutter and an increase in the wear of the cutter.

In addition, when the extruder is started, in order to make the cutter and the die plate closely contact without generating padding material, the initial feeding air pressure is set to 0.6 MPa in manual mode, and then the feeding air pressure is reduced by 0.01 MPa each time until when the feeding air pressure is 0.48 MPa, the automatic mode is enabled; during the process, the maximum current of the cutter is as high as 206A, which is about 30A higher than the normal value (see Figure 2).

When the rotation speed of the cutter increases, the force of the pelletizing water on the cutter to press the die plate increases (its effect is equivalent to increasing the feeding air pressure), and the number of frictions between the cutter and the die plate per unit time increases, so the cutter wears faster. It should be noted that when the cutter speed is too high, the cutter speed becomes the main factor affecting the cutter current. The cutter current increases obviously (see Table 1).

  • PP Grade

For different grades of PP, the physical properties are quite different. In general, the lower the MFR of PP, the greater the hardness of the molten material, the greater the friction on the cutting edge, and it is easier to passivate the cutting knife. In actual production, grade switching is often carried out according to market demand, and transition materials will be generated during the process of grade switching.

The MFR of the transition material continues to change, so the pelletizing process (water temperature, die plate temperature and barrel temperature, etc.) needs to be adjusted accordingly, so that the hardness change of the transition material passing through the barrel and the die plate is uncertain. Due to the change of the hardness of the transition material, the cutter is subjected to repeated action of alternating stress, resulting in passivation of the cutter.

  • Polymerization/Modification Process

For the same grade of PP, the MFR fluctuates within a certain range due to the characteristics of the polymerization/modification process. When the MFR fluctuates greatly, it is also unfavorable to prolong the life of the cutter. In actual production, due to the influence of changes in process and raw materials, such as fluctuations in the amount of additives added, inconsistent feeding, uneven catalyst preparation, and low purity of raw materials, the uniformity and stability of product properties may be affected, which is not conducive to Knife protection during granulation.

The fluctuation of the post-processing section of PP polymerization can also have an adverse effect on the properties of the powder. For example, due to the fluctuation of the steam in the drying unit of the polymer raw material, the drying effect is not good, so that the raw material contains a certain amount of water, and finally the knife wrapping phenomenon occurs in the pelletizer.

  • Others

Equipment factors include the flatness of the cutter plate, the perpendicularity of the cutter shaft and the die plate, the flatness of the cutter surface and the material of the cutter.

Improvement solutions

  1. Granulation process

During production, the feeding air pressure and the returning air pressure should be kept stable to avoid fluctuations. In order to ensure the quality of pelletize, sometimes need to maintain the feed air pressure, and when the cutter current is large, the retract air pressure can be slightly increased to reduce the cutter wear; it should be noted that the retract air pressure should not be too high Large, so as to avoid normal dicing when the production process fluctuates, which will eventually lead to the occurrence of knife padding and material sticking to the knife.

In the process, high feeding air pressure can increase the wear of the cutter, so frequent starting and stopping of the extruder should be avoided; At the same time, in the process of switching from manual mode to automatic mode, the feeding air pressure should be gradually reduced. If the setting value of the feeding air pressure drops suddenly, the adhesion force of the cutting knife to the die plate is instantly reduced, and more molten material is easy to punch out of the die plate, which can lead to padding and material sticking to the knife. At the same time, the cutting knife and the die plate must be coated with silicone oil before processing, so that the molten material sticking to the knife can be thrown away from the knife in time.

  • Material Grade

When granulating materials of the same grade, it is necessary to comprehensively adjust the temperature of the cutting water, die plate and the barrel to find the best combination of the three, so that the molten material has a suitable pelletizing hardness. In this way, the phenomenon of knife padding and material sticking to the knife caused by a large amount of molten material quickly punching out of the die plate can be avoided.

When changing the material, it is necessary to adjust the temperature of the cutting water, die plate and barrel according to the MFR trends, so that the molten material has a suitable hardness for cutting, to ensure a good appearance of the pellets. If there is tailing material, snake skin material, etc., it is necessary to adjust the granulation process in time according to the actual situation to avoid the occurrence of padding knife and material sticking to the knife (Table 2).

  • Process stability

Control the stability of front-end processes and equipment to ensure stable physical properties produced with the same formula, such as reducing feed fluctuations and adverse effects caused by uneven dispersion of additives and pigments, ensuring the purity of raw materials and keeping physical properties within a narrow range keep it steady.

Minimize the replacement of materials with a large MFR span, and optimize the modification process to reduce the generation of transition materials, so that they can quickly enter the qualified production stage, thereby reducing the adjustment time of the pelletizing process in the production of transition materials, which is conducive to cutter protection. In addition, ensure the normal operation of the material processing section and avoid wide fluctuations in the moisture content of the material.

  • Others

It is very important to ensure the installation accuracy of the cutter. The flatness of the cutter disc should be less than or equal to 0.01 mm, the perpendicularity of the cutter shaft to the template and the flatness of the cutter surface should be less than or equal to 0.03 mm.

By sharpening the knife, the flatness of the cutting disc, the perpendicularity between the cutting shaft and the template, and the flatness of the cutting surface can be improved to match the template. Therefore, the quality of the sharpening should be improved, and the feed air pressure should be reasonably controlled. and sharpening time to avoid knife damage during sharpening.

The material selection of the cutter is also very important. The hardness of the cutter should be lower than the hardness of the template to avoid the cutter from scratching the template. If the cutter frequently breaks, other high-quality cutters can be used or the cutter can be re-heated to eliminate the cutter. Defects in the texture of the material.

Regularly check the pH value of the pelletizing water. When the pH value is less than 7, open the fresh and refined water replenishment valve to make the pellet water overflow, so that the pelletizing water pH value is qualified, and other water such as industrial water shall not be added to the pelletizing water tank.

]]>
How to control pellet moisture with Underwater pelletizer? https://www.xindacorp.com/how-to-control-pellet-moisture-with-underwater-pelletizer/ Sun, 18 Oct 2020 05:58:00 +0000 https://www.xindacorp.com/?p=3837 In order to improve the quality of the finished product, some manufacturers have purchased underwater pelletizer, but found that the moisture content of the pellets still cannot come down.

In the production of plastic pellets, the cutting systems are mainly: cold strand cutting, hot air die face cutting, water ring cutting and underwater cutting, etc. The cutting method affects the water on the surface of the plastic pellets, and the water content directly affects the quality of the finished pellets. Among these cutting methods, the water content of underwater cutting method is relatively difficult to control.

So what are the factors that affect the water content of the finished pellets from underwater pelletizer?

1. The impact of the cutting blade Cutting blade in the application process will occur wear, when the blade wear to a certain extent, cutting pellets will take some burrs, these burrs adsorbed water in the subsequent drying process is difficult to remove, resulting in high water content.

2. The influence of the filter When the material comes out from the mold, the instant pressure release swells up, and the water is easily wrapped in the material and vaporized to form a hole, and the water contained in the material cannot be discharged through subsequent drying. 3. The mold pressure is too small Too small mold pressure makes the material extruded from the mold less dense, and the water infiltrates into the granule during the granule transfer process, and the infiltrated water is difficult to be taken out in the dewatering process.

4. Mismatch of dewatering machine / spin dryer The mismatched dewatering machine will easily cause the dewatering distance to be too short and the pellet climbing distance to be shortened during the dewatering process, so that the water cannot be removed smoothly.

5. Low water tank temperature As we all know, the efficiency of hot water dewatering is relatively higher than that of cold water, and even if we use the cold strand cutting method, the most effective way to dewater is to blow hot air. That is why the water content of the pellets is high when the machine is just turned on, because when the machine is turned on, the water in the tank enters the circulation system is too low, the temperature has to be reduced, and then the heat brought out from the pelletizer by the pellets to raise the temperature.

Will someone say: you can first raise the temperature of the water tank, so that the problem will be solved. To be honest, the water tank is slow to heat up, and even slower to cool down, I have tried, our pelletizer water tank to reduce the temperature of 1 ℃ takes about 7 minutes or so. Of course, by feeding cold water into the tank to cool down fast, but sometimes it is impossible to feed cold water. The tank water temperature is too low not only affects the dewatering efficiency in the dewatering machine, and because the water temperature is too low, it will affect the mold temperature, which brings the result that the head pressure is too high.

6. Water tank temperature is too high The water tank temperature too low is not good, then the water tank temperature high is good? Real practice has proved that the water tank temperature too high is not good, too high-water tank temperature let the particle cooling speed lower, easy to form craters on the surface of the pellets, at the same time, too high water temperature will bring the expansion of the pellets, with the gradual cooling of the pellet contraction, the water remains in the material.

7. The water in the tank is not enough Too little water tank water, easy to lead to slow down the water circulation process, pellets in the water soaking time is extended, inevitably have water infiltration, resulting in high water content of granules.

8. Unstable feeding The unstable feeding will easily cause the difference of cutting sizes in big range, and the big size difference will cause the big pellets to have more water on the surface.

Any other ideas, please share with us. (info@xindacorp.com)

Translated from Plaschain.

]]>
5 key points to keep the color masterbatch high speed mixing process correct https://www.xindacorp.com/5-key-points-to-keep-the-color-masterbatch-high-speed-mixing-process-correct%ef%bf%bc/ Sun, 18 Oct 2020 05:33:00 +0000 https://www.xindacorp.com/?p=3830 High-speed mixing is to put pigments, dispersants, carriers, etc. into a high-speed mixer for high-speed mixing according to the designed formula. It is an extremely important first production link in the production of color masterbatches.

Practical experience has proved that the pre-wetting of the pigment in the high-speed mixing process largely determines the final dispersibility of the color masterbatch product.

1. The quantity and rotation speed of the material carried by the high-mixing process

The high-mix loading capacity is related to the bulk volume of high-mix materials. Too much or too little loading will affect the normal operation of high-mixing, and it is difficult to achieve good high-mixing quality. The high-mixing speed is generally divided into two gears: low-speed start-up to reduce power load; high-speed mixing and moistening and discharging, with exceptions for special structures.

2. High mixing process temperature and time

If the high-mixing process does not have a certain temperature, it only plays the role of mixing at room temperature, and the initial wetting of the pigment cannot be achieved, and the key role of the high-mixing process is lost. There are two ways for the heat source of the high-mix process:

(1) To transfer the temperature through the high-mixer barrel oil heating, it is necessary to set the temperature control;

  • The temperature is transferred through the high-speed stirring and friction of the material, but the first pot of high-mixing takes a long time to accumulate the temperature.

The time required for high mixing is the time required for the material to “cook”—the dispersant melts and coats the carrier. It is related to the way of temperature transmission, the composition of materials, and the weather. The molecular weight of most dispersing and moisturizing agents is relatively small, and the more dispersing and moisturizing agents, the shorter the completion time of high mixing. Generally considered to be controlled at 15-30min. The abnormality of too long or too short time can promote the perfection of the formula, and finally the time required to reach the high mixing quality standard.

3.The high-mixing process requires careful observation. There are two ways to observe:

(1) A transparent observation port is provided to observe the changing state of the material at any time, but the transparent window is easily contaminated and affects the observation effect;

(2) Indirect judgment through current changes.

At the beginning of high mixing, due to inertia, the resistance is very large, and the power equipment is started with high load, causing the current to jump up instantly.After entering the normal constant speed operation, since the material is in a loose state and moves at a constant speed, the load of the power equipment is very light, and the current decreases accordingly. As the temperature increases, the dispersing wetting agent begins to melt gradually, and the adhesion state between the materials becomes more and more serious, which causes the motor load to increase. At this time, the current pointer gradually rises in a wave-like jitter.

4. High-mix quality judgment

After the high-mixing treatment, if the material is basically in the original loose state, there is a large amount of dry powder flying, which is generally judged as unqualified and needs to be reworked to continue high-mixing. If a large lump is formed, or even hardened at the bottom of the barrel, or if it is loose when discharging, and when it forms large lumps after being stored for several hours, it has to be stirred and broken again.

It is generally believed that the most ideal state is that there is basically no dust, and the overall appearance is roughly granular. The pigments are all wetted and then stick to the carrier. Even the largest particles can smoothly enter the screw granulation, which is the most ideal high mixing quality. In addition, special attention should be paid to the fact that the high mixing process is a process of wetting the pigment, and the wetting agent replaces the air and water on the surface of the pigment, so the removal of water should be considered to ensure the quality.

5. High-mix environmental protection requirements

High-mixed material pouring, stirring and discharging will generate certain dust and gas, which is the focus of environmental protection control.

At present, most enterprises install inverted funnel-shaped dust collection equipment above the high-mixing equipment, suck most of the dust and gas into the pipeline through suction, and transmit and filter the gas for treatment and release, and solid waste is collected and disposed of.

Source from Plaschain

]]>
The daily work of gravimetric feeder https://www.xindacorp.com/the-daily-work-of-gravimetric-feeder%ef%bf%bc/ Sun, 18 Oct 2020 05:33:00 +0000 https://www.xindacorp.com/?p=3833 How does the gravimetric feeder complete the feeding process?

There are many types of gravimetric feeder, including single screw gravimetric feeder, twin screw gravimetric feeder, and liquid gravimetric feeder. The feeding process can be divided into three steps:

1,When the gravimetric feeder is working, the material in its weighing hopper will gradually decrease with the operation of the machine. When the material reduces to the set weight, the feeding device will automatically start to replenish the material. At this time, the gravimetric feeder will work in a fixed speed mode. When the material increases to the set weight, it will stop feeding, and the equipment will automatically switch to the weightless mode.

2,The weighing sensor of the gravimetric feeder is linked with the weighing controller, and each item of data collected will be transmitted to the controller, and then the controller will perform calculations, and the calculation results will appear on the display screen. Through the data displayed on the display screen of the gravimetric feeder, we can not only view and monitor various data intuitively, but also control the working speed of the gravimetric feeder in time.

3,During the precise discharging process of gravimetric feeder, the control system will collect data at a high speed, and can calculate the reduced mass within a certain period of time to determine the speed and accuracy of the gravimetric feeder discharging.

What are the requirements of the gravimetric feeder for materials?

1,Gravimetric feeder have very high requirements for measurement accuracy, so the device composition of the equipment is designed for high precision. For example, during the entire operation process, the system is sealed, on one hand to ensure high precision, on the other hand, to prevent the material from polluting the environment, these measures are all related to the material. The gravimetric feeder is suitable for powdery or granular materials and liquid materials. Such materials have some features like easy to scatter, easy to stick, easy to adsorb, easy to volatilize, etc. Therefore, more attention should be paid in the process to meet different requirements.

2,In addition, for some chemical enterprises with special requirements, the loss-in-weight system also needs to have explosion-proof settings, which can meet the requirements of plant construction and national safety management.

3,The measurement of the gravimetric feeder is a combination of static measurement and dynamic detection. During use, there will be a series of parameters and time settings. In actual production, when there is a possible out-of-tolerance situation, an alarm function is set in the gravimetric feeder, which can effectively prevent the occurrence of problems.

]]>
Pay attention to the safe production of extruder https://www.xindacorp.com/pay-attention-to-in-the-safe-production-of-extruder%ef%bf%bc/ Wed, 14 Oct 2020 14:08:00 +0000 https://www.xindacorp.com/?p=3815

As the main equipment of compounding production, extruder bears the brunt of its operation difficulty and danger. Today, we will sort out the little common sense that you need to keep in mind during the operation and debugging of the extruder, and start small to protect safe and efficient production.

  1. Before starting the extruder, check whether there is any foreign matter in the barrel, up and down the hopper and inside, check whether the fastening bolts of each part are loose, whether the safety cover is firm, whether the position of each button switch is correct, and then lubricate each part. Add enough lubricating oil and do a good job of cleaning and sanitation of the equipment.
  2. Before starting the machine, check whether the temperature control is sensitive, whether the instrument is out of order, and whether the cooling water circuit is smooth. Usually, methods such as thermometer and cooling water are used for detection.
  3. Heat the screw, barrel and die head of the extruder according to the extruder operating procedures. After the temperature rises to the set temperature, it must be kept warm for about 10 minutes before starting the machine, so that the temperature of each part of the machine tends to be stable. .
  4. Notify staff around the device when you are ready to drive. Before starting the machine, be sure to tighten the connecting screws and bolts of each part of the die while it is still hot. Before the material is extruded, the operator must not stand in front of the die to prevent the bolt or screw from breaking and causing injury.
  5. Start the motor for driving the screw rotation at low speed, and check whether the pointer of the working ammeter of the main motor swings normally.
  6. The test run of the screw should not exceed 30 minutes. After everything is normal, connect the die head and the pelletizing equipment, install the connecting bolts for the die head, and apply a layer of molybdenum disulfide or silicone oil before use to facilitate disassembly.
  7. In the initial stage of feeding production, the screw should use the lowest working speed, and the feeding should be less and uniform. Check whether the pointer of the working ammeter of the motor used to drive the screw rotation changes at any time.
  8. After the extruder is put into normal production, the operator should always check the temperature change of the bearing part. When checking the temperature of the motor and each bearing part, gently touch the inspection part with the back of your finger. Do not touch any rotating parts with your hands during the operation of the equipment.
  9. When dismantling and installing the screw and mold, do not directly hit the parts with a heavy hammer, if necessary, pad hardwood and then tap to disassemble or install.
  10. When cleaning the residual material on the screw, barrel and mold, it must be cleaned with bamboo or copper knives, brushes, or professional water washing and air washing equipment to avoid scraping residual materials with steel knives or continuous use of fire. BBQ parts. Or use special screw cleaning material for cleaning without disassembly.
]]>